Posted By Aniket Yadav 07-20-2017 03:41 PM
Found In Egroup: Horizontal/Subsurface Infrastructure & Transportation
\ view thread
We used 100% class F fly ash as cementious replacement and we achieve strength more than 80MPa. But I am also very suspicious about future of fly ash based GPC. Because in India also government is reducing use of coal. So I also think that fly ash based GPC has no future now.